1. artifacts Qian processing alkali wash enough completely. 2. dyeing melt liquid temperature low. 3. dyeing solution surface has oil. 4. film layer not back net of rework products. 5. oxidation film was pollution. 6. oxidation Hou washing enough completely, not cleaning clean. 7. aluminum profile anode oxidation Shi current density had big. 8. anode oxidation solution temperature low, current density had small. 9. aluminum profile anode oxidation solution temperature high.